The five year sequence of fouling on 90-10 Cu-Ni (CA700) in seawater

Figure 13. Five year sequence of fouling on 90-10 Cu-Ni (CA700) in seawater

Photo at 3 months

Photo at 9 months

Photo at 18 months

Photo at 36 months

Photo at 48 months

Photo at 60 months