Fact 17 of 28
A copper strip barrier can keep snails and slugs from entering your garden. The slime they generate creates an electrical charge when contacting the copper and discourages the pests from crossing. Mount the strips around the perimeter of garden beds or containers, and be sure overhanging foliage does not provide an alternative path.