Almost half of all recycled copper scrap is old post-consumer scrap, such as discarded electric cable, junked automobile radiators and air conditioners, or even ancient Egyptian plumbing. (Yes, it's been around that long.) The remainder is new scrap, such as chips and turnings from screw machine production.