  • New Research on Runoff from Copper Roofs
    First report on the progress of research on how copper comes to be found in lakes, streams, and other bodies of water by the University of Connecticut, in collaboration with the International Copper Association Ltd, Copper Development Association Inc., and the Connecticut Department of Environmental Protection (Connecticut DEP).